Top Sale High Tear Resistance Rubber Carbon Black N220 Price Per KG Price For Rubber Industry
| Iodine Adsorption Number | 121±7 G/kg |
| Oil Adsorption Number(OAN) | 114±6 10-5m3/kg |
| Crushed OAN | 92-104 10-5m3/kg |
| Tint Test | 108-124% |
| CTAB surface area | 103-117103m2/kg |
| STSA | 99-113 103m2/kg |
| NSA | 107-121 103m2/kg |
| Heating Loss | ≤2.5 % |
| Pour Density | 360±40 G/M3 |
| 300% Modulus | -0.5±1.5 Mpa |
| Ash Content | ≤0.7 % |
| 45µm Seive Residue | ≤1000 Mg/kg |
| 500µm Seive Residue | ≤10 Mg/kg |
| Fine Content | ≤10 % |
Carcass,Conveyor belt,Hose,Rubber Shoes,Rubber Roller,Wire and cable,Rubber Products,Ink ,Coating,Plastic,Printing and dyeing